Nickel Based Vacuum Melted Superalloys

Tel:0086-510-88786098

E-mail: info@wxlongda.com

  • Nickel Based Super alloys
  • Nickel Based Super alloys Chemical Composition
Longda Super alloy company’s Nickel based super alloy bars, such as Inconel 713, Inconel 738LC, Inconel 718, Inconel 792, Inconel 939,Inconel 625, GTD 111,GTD 222 etc are very high purity, consistent quality and homogenized that satisfied to our customers home and abroad. Nickel based super alloys features and properties are as follows:

The nickel-based superalloys contain carefully balanced alloying additions of chromium, cobalt, aluminum, titanium and other elements.  Often components are produced by carefully controlled solidification in order to get an optimum directionally solidified or even single crystal structure.  These components can have strengths at 1000°C which exceed that of ordinary steels at room temperature.  They are essential in the hottest parts of gas turbines both for power generation and aircraft.

Nickel-based super alloys are found in a wide range of applications. The most prominent use is in the manufacture of gas turbines for use in commercial and military aircraft, power generation, and marine propulsion. Superalloys also find important applications in the oil and gas industry, space vehicles, submarines, nuclear reactors, military electric motors, chemical processing vessels, and heat exchanger tubing. Several generations of super alloys have been developed, each generation tending to have higher temperature resistance. 


Alloy Name

UNS No.

BS NO.

AMS

Rolls-Royce

GE

Snecma

Others

C1023




MSRR7046




C130


ANC12


MSRR7045




C242


ANC11


MSRR7217




C263


HC205


MSRR7040


DMD442-32


GTD111





B50A719



GTD111 DS





B50A858



GTD222





B50A850



GTD241





B50A972



GTD262





B50A985



GTD741





B50A973



Alloy X



5390

MSRR721




Hayness 230




MSRR7269



PWA1474

IN 100



5397

MSRR7047

C50TF107

DMD432-32


IN 600








IN 625



5401

MSRR7198

B50TF107


PWA1465

IN713C


HC203

5391

MSRR7164

B50TF16

DMD421.22

PWA655,PWA649

IN 713LC


HC209

5377

MSRR7048

B50TI239



IN 718



5383

MSRR7132

C5TF89

DMD423.32

PWA649,PWA1451

IN738C




MSRR7133,7125

B50A563A


PWA1451

IN738LC




MSRR7168,7173

B50A563B



IN792-5A




MSRR7169,7239




IN939







MTS1348,HXLM00424

MM002


HC207


MSRR7101,7080,7150




MM246


HC208


MSRR7061,7062




MM247







MTS1206

N75


ANC8


MSRR7004




N80


ANC9


MSRR1077




N90


ANC10


MSRR1789




PE10


ANC19


MSRR7184




PWA1056







PWA1056

PWA1188







PWA1188

PWA1422







PWA1422

PWA1432







PWA1432

PWA1437







PWA1437

PWA1440(SC)







PWA1440

PWA1455







PWA1455

PWA1467







PWA1467

PWA1475







PWA1475

PWA1483







PWA1483

Rene41



5399


B50TF37



Rene77





C50TF15

DMD437.32


Rene80





C50TF47


PWA1449

Rene125





C50TF60



Rene142





C50TF94



Rene220





C50TF91



Rene N2





C50TF121



Rene N4





C50TF75



Rene N5





C50TF122



Rene N6





C50TF114



Rene N500





C50TF129



Rene N515





C50TF130



SRR99




MSRR7210



MTS1162

RR2000




MSRR7225




U500



5384


B50A467



U700





B50A524


PWA656

WASPALOY







PWA1471

Alloy Name

AI

B

C

Nb

Co

Cr

Fe

Mn

Mo

Ni

Si

Ta

Ti

W

ZR

Others

C1023

4.10

0.006

0.15


9.7

15.5



8.0

Bal



3.6




C130

0.85


0.06



21.5



9.8

Bal



2.6




C242

0.15


0.31


10.0

21.0


0.35

10.5

Bal

0.35


0.2




C263

0.50


0.06


20.0

20.0



5.8

Bal

2.2




GTD111

3.00

0.10

0.10


9.5

14.0



1.5

Bal


2.8

4.9

3.8

0.01


GTD111 DS

3.00

0.10

0.10


9.5

14.0



1.5

Bal


2.8

4.9

3.8

<0.01


GTD222

1.20

0.10

0.10

0.8

19.0

22.5




Bal


1.0

2.3

2.0

0.02


GTD241

1.20

0.004

0.10


19.0

22.5




Bal



2.3

2.0

0.01

Nb+0.508Ta 1.3

GTD262

1.70

0.006

0.01


19.0

22.5




Bal



2.3

2.0

0.01

Nb+0.508Ta 1.35

GTD741

3.50

0.012

0.10


8.5

16.0



1.8

Bal



3.5

2.6

0.02

Nb+0.508Ta 1.8

Alloy X


0.800

0.08


22.0

18.5


0.50

8.5

Bal

0.08



0.6



Hayness 230

0.35

0.005

0.07



22.0


0.60

2.0

Bal

0.45



14.0



IN 100

5.50

0.015

0.17


15.0

9.7



3.0

Bal



4.7


0.04

V  0.9

IN 600



0.10



15.5

8.00

0.80


Bal

0.30






IN 625

0.20


0.05

3.6


21.5

3.00

0.20

9.0

Bal

0.20


0.2




IN713C

6.00

0.10

0.15

2.2


13.5

<2.00


4.2

Bal



0.8


0.07


IN 713LC

6.00

0.010

0.06

2.2


12.0



4.2

Bal



0.8




IN 718

0.60


0.06



19.0

Bal


3.0

52.5



0.9



Cb+Ta 5.0

IN738C

3.40

0.010

0.17

0.8

8.4

16.0



1.7

Bal


1.8

3.4

2.6

0.06


IN738LC

3.40

0.010

0.10

0.8

8.4

16.0



1.7

Bal


1.8

3.4

2.6

0.03


IN792-5A

3.40

0.015

0.08


9.0

12.6



2.0

Bal


4.0

4.0

4.0

0.03


IN939

1.90

01010

0.15

1.0

19.0

22.5




Bal


1.4

3.7

2.0

0.09


MM002

5.50

0.015

0.015


10.0

9.0




Bal


2.5

1.5

10.0

0.04

Hf 1.4

MM246

5.50

0.015

0.15


10.0

9.0



2.5

Bal


1.5

1.5

10.0

0.05


MM247

5.50

0.015

0.15


10.0

8.4



0.7

Bal


3.1

1.0

10.0

0.04

Hf 1.4

N75

0.20


0.12



19.5


0.60


Bal

0.60


0.4




N80

1.20


0.07



20.0


0.60


Bal

0.60


2.6




N90

1.20


0.09


16.0

20.0


0.60


Bal

0.60


2.6




PE10



0.04

6.7


20.0

3.00

0.30

6.0

Bal

0.25



2.5



PWA1056










Bal







PWA1188

3.40

0.025

0.05

0.9

20.3

13.0



3.8

Bal


2.4

3.7

2.1

0.05


PWA1422

5.00

0.015

0.14

1.0

10.0

9.0




Bal



2.0

12.0


1.6Hf

PWA1432

3.50

0.012

0.11


9.0

12.2



1.9

Bal


5.0

4.1

3.8

0.004


PWA1437

3.60

0.012

0.11


9.0

12.1



1.9

Bal


5.0

4.1

3.8

<0.02


PWA1440 (SC)

5.00

0.003/mx

0.04


5.0

10.0




Bal


12.0

1.5

4.0

0.03/mx

Hf 0.35

PWA1455

6.00

0.015

0.10


10.0

8.0



6.0

Bal


4.3

1.0


0.04

Hf 1.1

PWA1467

3.40

0.015

0.12


9.0

12.4



2.1

Bal


4.2

4.0

4.0

0.06

Hf 0.5

PWA1475

6.60

0.007

0.10



10.0



2.0

Bal


4.1


3.2

0.3

Hf 1.2

PWA1483

3.6

0.003/mx

0.07


0.9

12.2



1.9

Bal


5.0

4.1

3.8

0.0075/mx


Rene41

1.65

0.006

0.09


11.0

19.0



9.5

Bal



3.1




Rene77

4.30

0.015

0.07


15.0

14.7



4.2

Bal



3.4


0.04


Rene80

3.00

0.015

0.17


9.4

14.0



4.0

Bal



5.0

4.0

0.02


Rene125

4.8

0.015

0.11


10.0

8.9



2.0

Bal


3.8

2.4

7.0

0.04

Hf 1.6

Rene142

6.10

0.015

0.12


11.8

6.8



1.5

Bal


6.4

0.02/mx

4.9

0.03/mx

Hf 1.5, Re 3.0

Rene220

0.50

0.004

0.03

5.3

12.0

19.0



3.2

Bal


3.3

1.0




Rene N2

6.60

0.004

0.04


7.5

13.0




Bal

0.05

5.0

0.04 / mx

3.8

0.015/mx

Hf 0.1 , Re 1.6

Rene N4

4.20

0.004

0.06

0.5

7.5

9.8



1.5

Bal


4.8

3.5

6.0


Hf 0.15

Rene N5

6.20

0.004

0.05


7.5

7.0



1.5

Bal


6.5

0.04 / mx

5.0


Hf 0.15 , Re 3.0

Rene N6

5.80

0.004

0.05


12.5

4.2



1.4

Bal


7.2

0.04 / mx

6.0


Hf 0.15 , Re 5.4

Rene N500

6.60

0.004

0.04


7.5

6.0



1.5

Bal


6.6

0.04 / mx

6.3


Hf 0.15

Rene N515

6.30

0.004

0.05


7.5

6.0



2.0

Bal


6.5

0.04 / mx

6.3


Hf 0.6 , Re 1.5

SRR99

5.50


0.02


5.1

8.5




Bal


2..8

2.2

9.4



RR2000

5.50


0.015


15.0

10.0



3.0

Bal



4.0



V 1.0

U500

3.00

0.008

0.08


17.5

19.0



4.0

Bal



2.9




U700

4.30

0.020

0.80


15.0

15.0



4.5

Bal



3.3




WASPALOY

1.10

0.005

0.07


13.5

19.5



4.3

Bal


3.0



0.07


Leave Message
Please feel free to give your inquiry in the form below.We will reply you within 24 hours
Top
Product Catalog